Re: [MW:0] Conflict about heat available on electrode/work for the SMAW & GTAW process even having same polarity

Maulik,

It is not the conflict.

Pls understand the difference between the Thermionic & Non-Thermionic
cathodes,

That will explains the heat distribution. Pls go through the topic of Arc
Physics in ASM Welding Handbooks

Rgds,

K.Babu
Singapore


----- Original Message -----
From: "MAULIK" <mlkthakkar2@gmail.com>
To: "Materials & Welding" <materials-welding@googlegroups.com>
Cc: <bhavesh.patel@isgec.com>
Sent: Wednesday, August 18, 2010 1:47 AM
Subject: [MW:6549] Conflict about heat available on electrode/work for the
SMAW & GTAW process even having same polarity


> Dear all,
>
>
> 1. For SMAW-DCEN-2/3 heat to the electrode.

> 2. For GTAW-DCEN-2/3 heat to the work.

>
> Why this is conflict?
> Theoretically more heat is produced where the bombardment of electrons
> is carried out.
> Please give me clarification justification with proper evidence.
>
> Regards,
> Maulik H. Thakkar
> Welding engineer
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...