[MW:6569] Tube to tubesheet requirements

Dear All,
 
Could someone please specify the exact definition of root penetration gap for tube to tubesheets (QW193)? I have been evaluating many of them and have noticed that welders are using much more weld metal for joining them then required, i.e. client's design criteria. Isnt it lot of wastage of weld metal or its something beyond my comprehension? Secondly the design criteria for throat thickness as defined by customer is equal to tube thickness but I have seen a specification (probably some older version of ASME IX), which says that it is equivalent to 2/3 of tube thickness.
 
Can anyone please share his experience concerning above queries with T2Tsheets?
 
Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...