Why ASME sec VIII div.1 is silent of heat treatment above lower transformation temp.I mean normalising is not mentioned any where.
As per ASME sec VIII div.1 if due to cold forming fibre elongation is more that 5% then it gives reference of UCS-56,where it mention only stress releiving.
In which code I can find Normalising requirment(Temp, Holding time,loading temp)
I am aware that temp of normalising is about 910 Deg.c & holding time is 1mm/min.But I need reference of code.
Regards
Sachin
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Why ASME sec VIII div.1 is silent of heat treatment above lower transformation temp.I mean normalising is not mentioned any where.
As per ASME sec VIII div.1 if due to cold forming fibre elongation is more that 5% then it gives reference of UCS-56,where it mention only stress releiving.
In which code I can find Normalising requirment(Temp, Holding time,loading temp)
I am aware that temp of normalising is about 910 Deg.c & holding time is 1mm/min.But I need reference of code.
Regards
Sachin
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments