Skip to main content

[MW:6476] MW: 6458-P42 (Monel) to P1 (SA516 G.70) Welding

Hello Ibrahim,
 
A few queries  on your posting:-
  1. What's the design code
  2. What's the operating media? Does it involve HF or caustic environment in a refinery or Petrochemical Plant
  3. Are there any additional requirements- such as NACE  or API.
  4. What's the size of the nozzle to be welded?
  5. Is there any restriction from the client that "NO WELDING IS ALLOWED AFTER PWHT"
  6. Buttering on the nozzle opening with Monel(ER/E-NiCu7) + PWHT and installation and welding  of Monel nozzle could be an option. However in certain media this may be prohibited by the client/end user.
Appreciate your responses.
 
Thanks.
 
Pradip Goswami,P.Eng.
Welding & Metallurgical Engineer/Specialist
Ontario Power Generation Inc.
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Muhammed Ibrahim PK
Sent: Thursday, August 12, 2010 4:14 AM
To: materials-welding@googlegroups.com
Subject: [MW:6458] P42 (Monel) to P1 (SA516 G.70) Welding

Gents,
 
We have to weld a monel Nozzle SB165 (UNS N04400) (P No.42) to SA516G.70 (PNo.1) 45 mm thk
 
The vessel is required PWHT.
 
I need to qualify a PQR for this welding with ERNiCu+ENiCu-7.
 
Is it required to do PWHT of this joint (P42 to P1)?.
 
If PWHT is required what is the way of  welding of this joint?
 
If  PWHT is not required what is the procedure to weld it?
 
Is it required to butter the CS with monel before butt welding?
 
Is any post heting is required for this joint?
 

Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...