Good day

 

The Southern African Institute of Welding can provide the training required. If you require an official quotation, please let me have your company details etc.

 

Regards

John du Plessis

Technology Manager

 

Tel: +27 (11) 298 2100

Tel: +27 (11) 298 2103 (Direct)

Fax: +27 (11) 836 6014

Mobile:+27  (0) 82 883 4970

www.saiw.co.za

 

This email and any files transmitted with it are confidential and may be legally privileged. They are intended solely for the use of the individual or entity to whom they are addressed. Access to this e-mail by anyone else is unauthorised, and any disclosure, copying, distribution or other use of this e-mail is prohibited and may be unlawful. We will not under any circumstances have any responsibility or liability arising out of or in connection with any unauthorised use of this e-mail. If you have received this email in error please notify the sender before deleting it.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of skrie85
Sent: 10 August 2010 03:27 AM
To: materials-welding@googlegroups.com
Subject: [MW:6405] Welder Performance Qualification

 

Hi Sir,

I'm QC from fabrication company. But I need to give training to my staff and welder about the Welder Performance Qualification. Base material usually carbon steel, SS, Duplex and Super Duplex. Anybody can help me what the most important point about WQT to give them training? what should I focus on WQT to give them the training?

Thank you so much.

 

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...