dear all,can somebody give me a solution to get required tensile
strength of B7M bolts? I had tempered them first @700c for 1.5 hrs but
the UTS was only 630MPa,then again tempered them @700c for .5 hrs &
UTS was 662MPa. Hardness is ok-94HRB.
Regards,hari.
strength of B7M bolts? I had tempered them first @700c for 1.5 hrs but
the UTS was only 630MPa,then again tempered them @700c for .5 hrs &
UTS was 662MPa. Hardness is ok-94HRB.
Regards,hari.
--
K Harish Kumar, MTech
Consultant for:
Corrosion Metallurgy
Failure Analysis Surface Coating
Thin Films Vacuum Systems QMS.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments