Re: [MW:6060] Dual certification of material- valve & pipe- SS316/316L ??

 
Thanks you.
 
Does mill provide dual certify materials ???

On Wed, Jul 21, 2010 at 8:28 PM, Raghuram Bathula <raghurambathula@gmail.com> wrote:
simplest way is carbon content as per 316L grade and UTS/YS as per 316 grade will meet both the requirements.


On Wed, Jul 21, 2010 at 5:17 PM, Rana Vikas <vhrana@gmail.com> wrote:
Dear All,
 
Can you inform meaning of dual grate certification material ??
 
Also send properties of SS316/316L
 
One of our client specification mentioned that piping & valve material should be dual certified i.e SS316/316L .
 
Early reply is appriciable


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...