HI,
 
Generally, if you use drum-packed flux, you do not need re-drying before opening the drum.
 
but if you are requested to bake the F7A6 flux, you may refer to below suggestion:

300-350℃     2h-10h

 

Best regards

 

Roy LIU

 

Böhler Welding Group - China

you may contact me via roy.liu@bw-group.com.cn

 
> Date: Wed, 21 Jul 2010 02:17:27 -0700
> Subject: [MW:6049] SAW FLUX BAKING
> From: ajay.m.appukuttan@gmail.com
> To: materials-welding@googlegroups.com
>
> Hello ,
>
> What are the flux baking requirements incase of saw F7A6 flux (SFA
> 5.17). The product website(Lincoln) says there is no baking requirment
> in case of unopened flux, how ever does any one know of any asme code
> requirements.
>
> Regards
>
> Ajay M. Appukuttan
> Q.C Inspector (Welding , Painting & Ndt)
> Oman Metal Industries
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


使用Messenger保护盾V2,支持多账号登录! 现在就下载!

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...