Adi,
        There is difference in chemical composition like Manganese contenet is more in case of LTCS compare to CS to enhance impact properties.
 
Regards,
vaithiyanathan.
On Mon, Jul 19, 2010 at 2:49 PM, Adi <adinraos@gmail.com> wrote:
Dear all



I have a question regarding carbon steel. What is the difference of
LTCS (low temperature carbon steel) from CS? Someone told me that the
composition of the two just the same and LTCS is only impact test is
done, is it correct?



Regards

Adi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Best Regards

B.Vaithiyanathan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...