U can give mini. 10 deg. in WPS for CS pipe, for WT upto 25.4mm. 

On Sat, Jul 17, 2010 at 9:08 PM, shibu simon <shibusimon2000@yahoo.co.uk> wrote:
Dear all,

Carbon steel base metal initial temperature was 32 deg celcius, during PQR qualification as per API 1104. Decreasing pre heat temperature is an essential variable as per API 1104. So what minimum preheat temperature to give in WPS.

Thanks.

shibu simon




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards
AAKARSH PP
QA/QC-Welding
LTCS Shop-Hyundai Engg. & Construction
Karan Gas Field Development Project

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...