Dear Nilesh ,
   
                   After Purging plz give some time to demolish the atmosphere air. and check whether any impurities present inside the pipe and near the weld joint. close the both end of pipe with some closer. one end is supplied by purging hose and another end you make a fine hole to have a flow of the purging gas outside. If you close the welding portion from outside 75% other than the welding it will be better. other than that you better check other specifications as mentioned other mails.
 
Regards,
J.C.Andrews
QA/QC Engineer
Doha-Qatar.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...