RE: [MW:5988] Problem wk\hile root run

What is the material, joint details, backing gas delivery & retention
method, welding position, welder's previous experience? I assume GTAW.

BR
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Muhammed
Ibrahim PK
Sent: 15 July 2010 14:21
To: materials-welding@googlegroups.com
Subject: Re: [MW:5986] Problem wk\hile root run

change the purging to 6-8 ltr.
reduce the root gap

Thanks & Regards
Muhammed Ibrahim PK


On 15 July 2010 10:27, waman nilesh <wamannp@gmail.com> wrote:


I have problem while doing root run the weld get black from
backside as we have maintain the backing 10 lpm & Shielding 12 lpm as
per WPS.
Can anybody tell me the reason & how to avid it.

Nilesh

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel
views and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...