I can give rough idea about S355J2G3
S:- Structural Steel
355:- Yield Strength
J2:- 27 J @ -20º C
G3:- Delivery Condition-Normalized.
Please see the attachment having password jigs
Thanks

On Tue, Jul 13, 2010 at 10:12 PM, ASME <vettaikkaran2011@gmail.com> wrote:
Dear,

Note that materials No 1.429 & 1.4740 arn't cast iron,

Material Number
1.4729

Steel group
Stainless and heat-resisting steels

Symbol
GX40CrSi13

Standards
?NORM EN 10295 (10/2002)
Heat resistant steel castings

Range of application
Heat-resisting steel castings:
Hearth-plates, door frames and other similar hearth parts.
Suitable welding filler materials 1.4733, 1.4829.

Material Number
1.4740

Steel group
Alloy special steels: Heat resistant steels with < 2,5% Ni

Symbol
GX40CrSi17

Standards
DIN EN 10295 (01/2003)
Heat resistant steel castings
International conformity
EN 10295 (2002)
Replaces
DIN 17465 (08/1993)

Range of application
Heat-resisting steel castings:
Superheater parts, pipe clamps, carrying handles, grates.
Suitable welding filler materials 1.4015, 1.4502, 1.4829.

Material Number
1.1191

Steel group
Non alloy special sructural steels: Structural steels with average C <
0,50%

Symbol
C45E; Ck 45 †

Standards
DIN EN 10083-1 (10/1996)
Quenched and tempered steels. Special steels.
International conformity
EN 10083-1+A1 (1996)
Replaces
DIN 17200 (03/1988) (03/1987)

DIN EN 10132-3 (05/2000)
Cold-rolled narrow steel strip for heat-treatment. Steels for
quenching and tempering.
Replaces
EN 10132-3 (2000)

DIN EN 10250-2 (12/1999)
Open die steel forgings for general engineering purposes. Non-alloy
quality and special steels.
Replaces
EN 10250-2 (1999)

DIN EN 10269 (11/1999)
Steels and nickel alloys for fasteners with specified elevated and/or
low temperatures properties.

DIN EN 10277-5 (10/1999)
Bright steel products. Steels for quenching and tempering.

DIN EN 10297-1 (06/2003)
Seamless circular steel tubes for mechanical and general engineering
purposes. Non-alloy and alloy steel tubes. Non-alloyed high-quality
steels

DIN EN 10297-1 (06/2003)
Seamless circular steel tubes for mechanical and general engineering
purposes. Non-alloy and alloy steel tubes. Alloyed quality steels

DIN EN 10305-1 (02/2003)
Steel tubes for precision applications. Seamless cold drawn tubes.

DIN SEW 550 (08/1976)
Steels for larger forgings.

Range of application
Heat-treatable steels:
Automobile- and motor construction, mech. engineering

High-temperature constructional steels:
Bolts and nuts, resistant to elevated temperatures up to 400 °C

These steels can also be supplied with a sulphur-content of
0,020-0,040%. Then e.g. C22E = C22R, resp. Ck22 = Cm 22 or receive the
letter S (e.g. 32Cr2 = 32CrS2). Number of material in brackets. The
mechanical properties are identical.

Material Number
1.0570

Steel group
Non alloy quality steels: Steels with average C > 0,25 < 0,55 % or Rm
> 500 < 700 N/mm²

Symbol
S355J2G3; St 52-3; St 52-3 G; (S355J2G3+CR)

Standards
DIN 1623-2 (02/1986)
Steel flat products. Cold reduced sheet and strip. General structural
steels.
International conformity
ISO 4997 (1999)

DIN 5512-1 (05/1997)
Materials for rail vehicles. Structural steels and structural steels
with improved atmospheric corrosion resistance, hot rolled.

DIN 5512-2 (05/1997)
Materials for rail vehicles. Unalloyed steels for cold rolled flat
products up to 3 mm thickness.

DIN 5515 (11/1978)
Steel sections, bars and flat products of non-alloyed steels and
general structural steels. Summary for rail vehicles.
Replaced by
E DIN 5515 (10/1999)

DIN EN 10025 (03/1994)
Hot rolled products of non-alloy structural steels.
Replaced by
EN 10025 (1993); ISO 630 (1995); ISO 4995 (2001); ISO/FDIS 6316
(2000); ISO 13976 (1998)

DIN EN 10250-2 (12/1999)
Open die steel forgings for general engineering purposes. Non-alloy
quality and special steels.

Way of deoxydation: Fully killed steel containing nitrogen binding
elements in sufficient amounts to bind the nitrogen (p.e. Al >=
0,02%).
With special cold workability: 1.0569; S355J2G3C
Former designation DIN 17100: St 52-3 N
Former designation of steels with special working properties,
Cold flanging: 1.0573; QSt 52-3 N
Cold drawing: 1.0597; ZSt 52-3 N
Cold roll forming: 1.0575; KSt 52-3 N

Material Number
1.0569

Steel group
Non alloy quality steels: Steels with average C > 0,25 < 0,55 % or Rm
> 500 < 700 N/mm²

Symbol
S355J2G3C; QSt 52-3

Standards
DIN 5512-1 (05/1997)
Materials for rail vehicles. Structural steels and structural steels
with improved atmospheric corrosion resistance, hot rolled.

DIN EN 10025 (03/1994)
Hot rolled products of non-alloy structural steels.
International conformity
EN 10025 (1993); ISO 630 (1995); ISO 4995 (2001); ISO/FDIS 6316
(2000); ISO 13976 (1998)
Replaces
DIN 17100 (01/1980)

DIN EN 10277-2 (10/1999)
Bright steel products. Steels for general engineering purposes.

Material Number
1.0576

Steel group
Non alloy quality steels: Steels with average C > 0,25 < 0,55 % or Rm
> 500 < 700 N/mm²

Symbol
S355J2H; RoSt 52-3

Standards
DIN 1626 (10/1984)
Welded circular unalloyed steel tubes subject to special requirements.
International conformity
ISO 9330-1 (1990)
Replaces
DIN 1626-1 (01/1965); DIN 1626-3 (01/1965)

DIN EN 10210-1 (09/1994)
Hot finished structural hollow sections. Non-alloy steels

DIN EN 10219-1 (11/1997)
Cold formed welded structural hollow sections. Fine grain steels

Material Number
1.0976

Steel group
Alloy quality steels: Steels for various applications

Symbol
S355MC

Standards
DIN EN 10149-2 (11/1995)
Hot rolled flat products made of high yield strength steels for cold
forming. Delivery conditions for thermomechanical rolled steels.
International conformity
EN 10149-2 (1995); ISO 5951 (2001); ISO 6930-1 (2001)

Range of application
Fine grained steels for cold pressing:
Longitudinal beams
Construction of frames
Parts for cold pressing
Cold rolled sections



On Jun 11, 10:25 am, limesh M <limes...@gmail.com> wrote:
> Dear All,
>
> I am in urgent need of theequivalentstandards of the following
> materials(From which standards these designated materials came) for
> chemical composition and traceability.Please help me .
>
> Cast Iron                       1.4729
>
> Cast Iron                       1.474
>
> Flat Iron                        C45K
>
> Cast Iron                      ENGJL250
>
> Cast Iron                      ENGJL250+1.5% CR
>
> Shaft                            S355J2G3
>
> Shaft                            S355J2G3+C
>
> Pipe                             S355J2H
>
> Steel Plate                   S355MC
>
> M16 Hex Bolt               DIN 916
>
> 17 Washer                   DIN 7349
>
> Refractory                    Alocast H 40
>
> Thanks &Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...