The following is the range qualified for the deposited weld metal as per QW 451.1, ASME Sec IX
GTAW - 1.5 mm to 7.0 mm max (2t),
MMAW - 1.5 mm to 19.6 mm max(2t),
Where t= deposited weld metal thickness,
Regardless the base metal thickness.
Note: Stephen should mention the base metal thickness.
The deposited weld metal thickness can be recorded on the WPS wrt the base metal thickness and deposited weld metal thickness for the said PQR.
On Fri, Jul 9, 2010 at 9:31 AM, Ankur Mande <prince.ankur@gmail.com> wrote:
Stephen,The following is the range qualified for the weld metals.GTAW - 7.0 mm maxMMAW - 19.0 mm maxAnkur.On Fri, Jul 9, 2010 at 5:06 AM, Stephen Milne <sim@aalborg-industries.com.au> wrote:
--Hi,
Have the following question regarding weld metal deposition on PQR with combined GTAW & MMAW processes.
Have recorded both GTAW = 3.5mm & MMAW = 9.8mm onto PQR (QW-204b) but unsure of the ranges qualified
for both and should they be recorded on associated WPS.
Thanks
QA/QC
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment