RE: [MW:5892] PWHT Requirement of carbon steel (BS EN 10025 S275JR) plate 25mm to the plate (ASTM A387 Gr 11 Cl 2) 18mm THK
Construction Code is Section VIII Division 1.
Weld Geometry: Groove + Fillet.
Best Regards,
Dharmesh Mistry
HEURTEY PETROCHEM
Tel. +91 22 67740074
Cell +91 98207 35814
Dharmesh.Mistry@heurtey.in
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bathula Raghuram (Mumbai - PIPING)
Sent: Wednesday, July 07, 2010 5:10 PM
To: 'materials-welding@googlegroups.com'
Subject: RE: [MW:5891] PWHT Requirement of carbon steel (BS EN 10025 S275JR) plate 25mm to the plate (ASTM A387 Gr 11 Cl 2) 18mm THK
What is your construction code? , weld geometry is it butt or fillet?
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Dharmesh Mistry
Sent: Wednesday, July 07, 2010 4:57 PM
To: materials-welding@googlegroups.com
Subject: [MW:5889] PWHT Requirement of carbon steel (BS EN 10025 S275JR) plate 25mm to the plate (ASTM A387 Gr 11 Cl 2) 18mm THK
Dear all,
Is it required to do PWHT for fillet weld carbon steel (BS EN 10025 S275JR) plate 25mm to the plate (ASTM A387 Gr 11 Cl 2) 18mm THK?
Best Regards,
Dharmesh Mistry
HEURTEY PETROCHEM
Tel. +91 22 67740074
Cell +91 98207 35814
Dharmesh.Mistry@heurtey.in
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments