Tuesday, July 6, 2010

RE: [MW:5869] Select Filler Rods For Welding Similar & Dissimilar Metals

You may refer the attachment for dissimilar combination, and you can get a copy of complete welding manual from http://www.boehler-welding.com/, due to space constraint I am not posting it in the group

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Chella
Sent: Tuesday, July 06, 2010 10:02 AM
To: Materials & Welding
Subject: [MW:5868] Select Filler Rods For Welding Similar & Dissimilar Metals

Dear Members,

I am involved in maintenance of Boiler pressure parts, kindly help me by providing some sort of ready reckoner for selection of filler rods for welding similar & dissimilar metals. Eg. SA 210 GrA1 to SA 210 GR A1, SA 213 T11 to SA 213 T22, SA213 T22 to SA 335 P22.

With Regards,

Chella


Filtered by Hosted Filtering

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...