Re: [MW:5850] STRESS RELIEVING REQUIREMENT

It is required for all P1 material >20mm, irrespective of fluid service.

On Sun, Jul 4, 2010 at 5:54 PM, <desaid@toyoindia.com> wrote:

Hello,

As per ASME B31.3; for CS material PWHT requirement is above 20mm.
Is this applicable to category D fluid service class also?

Or code has given liberty to skip PWHT for category D fluid service even though thickness is greater than 20mm.

Pls. advise.

Thanks in advance,

Thanks & Regards,
Dhwani Desai
Planning & Piping Dept.
Ext.-7681


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...