Saturday, July 3, 2010

RE: [MW:5839] API 650 requirements guidance

Please find the attachment for the API requirements and acceptance. (except RT)

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of AGUSTIN JIMENEZ
Sent: Friday, July 02, 2010 1:03 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:5818] API 650 requirements guidance

 

Hi Rajneesh.

Read API 653 INSPECTION, REPARATION, ALTERATION AND RERATING OF TANKS, APPENDIX C.

BEST REGARDS

AGUSTIN JIMENEZ

 


De: Rajneesh Gaur <rajneeshgaur@gmail.com>
Para: materials-welding@googlegroups.com
Enviado: mié, junio 30, 2010 6:37:40 AM
Asunto: [MW:5804] API 650 requirements guidance

Dear all,
I need some guidance about the tolerances, critical aspects of
inspections as per requirements of API 650.
Kindly guide with relevant material and references.
Regards
Rajneesh gaur

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


 

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...