Re: [MW:5829] 6GR qualified welder. As per AWS D1.1

6GR qualified welder can weld single sided weld provided weld joint shall have backing strip or backing.






On Fri, 02 Jul 2010 22:31:40 +0530 wrote
>



Hello
gents,



I
have a query on butt joint welding with 6GR qualified welder. As per AWS D1.1
(2006) Table 4.10 Note d, 6GR qualified welder is qualified for all position.
However, they are not qualified to weld production weld butt joint welded from
one side without backing or welded from both side without backing. In this
case, it is considered as single side welding without backing. Pls could some
one in the house clarify more on these if I am right or wrong as per D1.1 interpretations?












Regards





Philip Taiye

Principal QA/QC Welding Engineer

(MIPs
Quality Control)

DeltaAfrik
Engineering Limited

2nd
Floor, City Express Bank Building

Plot
1637 Adetokunbo Ademola Street

Victoria
Island, Lagos Nigeria

Phone: +234-1-461-8508, +2341-461-6137 ext. 1257

Cell: +234-(0)-803-803-1396

Fax: +234-1-262-2418

e-mail: taiye.philip@worleyparsons.com













*** WORLEYPARSONS GROUP NOTICE ***
"This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it.
If you have received this email in error, please notify us immediately by return email and delete the email and any attachments.
Any personal views or opinions expressed by the writer may not
necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."







--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>



John Rodrigues

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...