Thursday, July 1, 2010

Re: [MW:5816] Jacket TKY tack welds

Dear sreevalsan
 
bullet tacking is preffered refer the client specification. check client fabrication procedure
 
rgds
m.m.reddy

On Wed, Jun 30, 2010 at 5:07 PM, sreevalsan sreedharan <sreevalsan68@gmail.com> wrote:
Dear All
 
In Jacket TKY joint fabrication which types of tack welds are commonly used and where I can get tack welding details  
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
THX & RGDS
M.M.REDDY
QA/QC INSPECTOR (MECHANICAL)
METHANOL PLANT
DAMIATTA - EGYPT
0020168194532

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...