Re: [MW:5815] Hard-facing overlay versus Corrosion resistent overlay

Hi,
 
corrosion resistant overlay applying to prevent corrosion of equipment when corrosive chemical service.
hard facing overlay applying to prevent wear when contact with another metal. eg. bearings, wear plate.

Thanks & Regards
Muhammed Ibrahim PK



On 1 July 2010 16:40, Fernando Gameiro <fgameiro@velan.pt> wrote:

Dear All,

 

According to ASME IX the difference between Hard-facing overlay and Corrosion resistant overlay is limited to the type of tests that is required on PQR and WPS ?

 

According to ASME, how to define if certain overlay is a Corrosion resistant or a Hard-face?

 

Thanks

 

Fernando Gameiro

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...