Friday, July 16, 2010
[MW:5994] PSL 1 and PSL 2
Dear All
Can you tell the difference between PSL 1 and PSL 2 specification levels as per API 5L.
Thanks and Regards
Harikrishnan N S
QA/QC Engineer
Punj Lloyd Ltd
Mob.No. : +91 9769305625
They can, because they think they can.......
---------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------
This e-mail and any files transmitted with it are for the sole use of the intended recipient(s) and may contain confidential and privileged information. If you are not the intended recipient of this communication, we request you to notify the sender immediately by return email and destroy all copies and the original message. Any unauthorized review, use, disclosure, dissemination, forwarding, printing or copying of this email is strictly prohibited. The recipient acknowledges that Punj Lloyd Limited or its subsidiaries and associated companies (collectively "Punj Lloyd Group") are unable to exercise control or ensure or guarantee the integrity of/over the contents of the information contained in e-mail transmissions and further acknowledges that any view, opinion or advice expressed in this message are those of the individual sender and no binding nature of the message shall be implied or assumed unless the sender does so expressly with due authority of Punj Lloyd Group. Although we have taken all reasonable precautions to ensure that this communication is free from viruses. We do not assume responsibility for any loss or damage arising from the use of this email.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point
Dear Experts. If anyone having presentation of WPS,PQR and WPQ as per ASME SEC.IX in power point then please share . Regards Sanja...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment