General composition of  both the alloys are as follows.For sea water applications both the alloys are popular.Alloy C-63000(Ni-Al bronze) is an alloy with higher strength which could be attractive from design point of view and would be costlier than the other variety.
 
 
 
 
 
You may find the attached booklet as good information to start with.

Bronze alloys are  common cost effective choices in sea water applications, many times as castings. However if heat exchangers are to be fabricated entirely from this alloy, it would involve good fabrication practices.

Thanks.

Pradip Goswami,P.Eng.
Welding & Metallurgical Engineer/Specialist
Ontario Power Generation Inc.
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Phirke, Praphulla D (GE Oil & Gas)
Sent: Saturday, July 10, 2010 3:13 AM
To: materials-welding@googlegroups.com
Subject: [MW:5927] Copper Base alloys
Importance: High

Dear all,
For one of my project, I have to use Sea water for cooling purpose.
For the same customer has suggested following materials for heat exchanger
 
Shell, Channel, Channel cover & Baffles as ASTM B 171 C61400 or ASTM B 171 C63000
 
I never used such type of materials earlier.
 
Can anyone suggest me which option is best option & why?
Also let me know which is costlier ?
 
Thanks
Praphulla
 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...