Monday, July 5, 2010

[MW:5863] Nozzle welding inspection in 100 degrees by UT-reg

Dear All,Our customer wants to check the Nozzle welding to shell with reiforcement pad by UT.The current working temperature on the vessel is 100 degree celsius and they are not ready to shutdown.They need to check the nozzle welding to shell and padplate welding to nozzle with the current working temperature.We explained them that with this temp.we UT can not be done also without removal of Reiforcement pad shell to nozzle welding cannot be examined by UT.
Does any one know how to check this joint with the current working temperature.Is there is any special technique or mehod to check this?
 
Regards,
 
(Karthik)

Karthikeyan.S
 
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...