Sunday, July 4, 2010

[MW:5852] Re: STRESS RELIEVING REQUIREMENT

Still you need go by your design code and follow whichever is
stringent.

On Jul 4, 6:09 pm, des...@toyoindia.com wrote:
> <Security Level 2>        
> Thank you. Even our understanding the same.
>
> But, in our project for various piping classes Licensor's / PMC
> specifications specify the PWHT requirement.
> Four variables are being use.
>
> For Process Carbon Steel Piping class : PWHT : As per ASME B31.3 (That
> means above 20mm thickness)
> For all NACE Service piping classes (Carbon Steel) : PWHT : YES  (that
> means for all thickness unlike code)
> For Steam service class : PWHT : IBR (we concluded similar to B31.3)
> For all Alloy steel Piping class : PWHT : YES (that means for all
> thickness unlike code)
> For certain steam service class PWHT : As per ASME B31.1 (That means above
> 20mm thickness)
>
> For Category "D" fluid service Piping class : PWHT : NO (hence, the
> question)
>
> Not able to interpret the philosophy.
>
> Thanks & Regards,
> Dhwani Desai.
> TOYO - PLANNING & PIPING DEPT.
> 91-22-2573 7681.
>
> Raghuram Bathula <raghurambath...@gmail.com>
> Sent by: materials-welding@googlegroups.com
> 07/04/2010 06:24 PM
> Please respond to
> materials-welding@googlegroups.com
>
> To
> materials-welding@googlegroups.com
> cc
>
> Subject
> Re: [MW:5850] <Security Level 2>STRESS RELIEVING REQUIREMENT
>
> It is required for all P1 material >20mm, irrespective of fluid service.
>
> On Sun, Jul 4, 2010 at 5:54 PM, <des...@toyoindia.com> wrote:
>
> Hello,
>
> As per ASME B31.3; for CS material PWHT requirement is above 20mm.
> Is this applicable to category D fluid service class also?
>
> Or code has given liberty to skip PWHT for category D fluid service even
> though thickness is greater than 20mm.
>
> Pls. advise.
>
> Thanks in advance,
>
> Thanks & Regards,
> Dhwani Desai
> Planning & Piping Dept.
> Ext.-7681

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...