Dear All
 
We need to weld following pipe material
 UTS 845/855 Mpa,
 T.S. - 990/1000Mpa
 Chemical Comp. - 0.35C, 0.65Mn, 0.20Si, 0.95Cr., 0.18Mo
 
Can anybody advise suitable consumable for this application
 
Thanks
 
 
 
 

--