Hi All,
Greetings...!
For Weld Scanning in UT (Single V - plate or pipe) , we have some formulas to find the Skip Distance , Beam Path Like that...Using them we can calculate the depth of defect and can proceed further.
Is this same thing for Double V joints? or Anything Different. Please guide me the same.
Can you peoples send me the clear echo pattern system in UT of soft copy and how to locate/calculate the discontinuity exactly in the weld asap?
Expecting reply asap.
Thanks
Kamaraj
India.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point
Dear Experts. If anyone having presentation of WPS,PQR and WPQ as per ASME SEC.IX in power point then please share . Regards Sanja...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...