Dear All,
Good Morning
I have query regarding the solidification Cracking.
Generallly, FeS the compound responsible for solidification cracking. Also Arsenic, Sulphur shows same phenomenon.
Now Delta- Ferrite in 3-8 FN proportion prevents hot cracking.
But how ?? In most of the books, it is written that, " Delta- Ferrite has tendency to lock the impurities".
But how Delta- Ferrite can be helpful for the prevention of hot cracking by locking the impurities??
Also, what happens if Delta- Ferrite is very low of the order of 0.5 FN or so or what happens if Delta-Ferrite is high of the order of 15 FN or so.
 
 
Dear All,
Please help me to find the answers.
 Thanks in advance.
 
Jignesh
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...