Sunday, June 20, 2010

Re: [MW:5673] Ferrite content variation with PWHT time

ya, § ferrite varies with soaking time but more dependent on the
cooling rate also.

On 6/20/10, P.Rao <vasantharao2009@rediffmail.com> wrote:
>
>
> Dear all,
>
> Is it Delta ferrite number/value in stainless welds/Overlay will varies with
> PWHT soaking time?.
>
> regards
> P.Rao.
> 0966543636485
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
K Harish Kumar, MTech
Consultant for:
Corrosion Metallurgy
Failure Analysis Surface Coating
Thin Films Vacuum Systems QMS.

www.itindt.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding