Hi
I understand that welder position in WPS is not essential, I think that you can qualify in other position in WPQ, but later of qualify to welder not can change position to WPQ here if is essential.
Ed my friend what you opinion?
Agustin Jimenez
De: john rodrigues <johnrodrigues2@rediffmail.com>
Para: materials-welding@googlegroups.com
Enviado: jue, junio 17, 2010 4:28:31 AM
Asunto: Re: [MW:5634] WPS /WPQR
Mr. Afzal,
Good afternoon,
With reference to AWS D1.1, table 4.1, you cannot use this procedure for welding in 3G position.
Thus, you cannot qualify welder by using WPS which is qualified in 4G position.
Regards.
JohnR
On Thu, 17 Jun 2010 12:51:02 +0530 wrote
>Good morning Group,
I have a qualified WPS inover head position to AWS D 1.1 requirements. Now I want to use this approved WPS ( Over head position ) to qualify a welder in 3 G( Vertical Up hill) position to AWS D 1.1 requirements.
Can I use the WPS or do I need to qualify a WPS in 3 G Position with reference to AWS D 1.1 requirements.
Mohammad Afzal Baig
````````````````````````````````````````` email:afzal1972@gmail.com
--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
John Rodrigues
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
De: john rodrigues <johnrodrigues2@rediffmail.com>
Para: materials-welding@googlegroups.com
Enviado: jue, junio 17, 2010 4:28:31 AM
Asunto: Re: [MW:5634] WPS /WPQR
Mr. Afzal,
Good afternoon,
With reference to AWS D1.1, table 4.1, you cannot use this procedure for welding in 3G position.
Thus, you cannot qualify welder by using WPS which is qualified in 4G position.
Regards.
JohnR
On Thu, 17 Jun 2010 12:51:02 +0530 wrote
>Good morning Group,
I have a qualified WPS inover head position to AWS D 1.1 requirements. Now I want to use this approved WPS ( Over head position ) to qualify a welder in 3 G( Vertical Up hill) position to AWS D 1.1 requirements.
Can I use the WPS or do I need to qualify a WPS in 3 G Position with reference to AWS D 1.1 requirements.
Mohammad Afzal Baig
````````````````````````````````````````` email:afzal1972@gmail.com
--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
John Rodrigues
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment