Thursday, June 17, 2010

Re: [MW:5634] WPS /WPQR

Mr. Afzal,
Good afternoon,
With reference to AWS D1.1, table 4.1, you cannot use this procedure for welding in 3G position.
Thus, you cannot qualify welder by using WPS which is qualified in 4G position.
Regards.
JohnR

On Thu, 17 Jun 2010 12:51:02 +0530 wrote
>Good morning Group,
I have a qualified WPS inover head position to AWS D 1.1 requirements. Now I want to use this approved WPS ( Over head position ) to qualify a welder in 3 G( Vertical Up hill) position to AWS D 1.1 requirements.

 
Can I use the WPS or do I need to qualify a WPS in 3 G Position with reference to AWS D 1.1 requirements.
 
 

Mohammad Afzal Baig
````````````````````````````````````````` email:afzal1972@gmail.com
       


 
     




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>



John Rodrigues

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...