Hello Jhon
 
Yes, we are doing inspection of a church structures and need know how many is the thickness loss that i can accept.
 
Agustin


De: john rodrigues <johnrodrigues2@rediffmail.com>
Para: materials-welding@googlegroups.com
Enviado: mié, junio 16, 2010 4:19:52 AM
Asunto: Re: [MW:5613] structures acceptance criteria for loss of thickness

Austin,
May I know what is application of structure?
Regards.
JohnR

On Wed, 16 Jun 2010 08:53:04 +0530 wrote
>Dear colleagues, I have a query them.
>
>For the inspection of tubular structures (section square or rectangular), which is the acceptance criteria for loss of thickness and standard that applies? . This structure is 12 years old, made in the open.
>
>Many would know thank
>
>Greetings,
Agustin
>
>











--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>



John Rodrigues

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...