Wednesday, June 16, 2010

Re: [MW:5608] Tube to tube sheet welding

Hi,
 
It is the minimum depth of the weld where weld will withstand the load. If it is agroove cum fillet weld the distance of weld from botom of groove to top of fillet.
 
Regards,
Ibrahim

On 16 June 2010 00:18, Shadab Alam Ansari (Welding Engineer) <shadabansarialam@gmail.com> wrote:
In Tube to tube sheet weld joint what is the minimum leak path
distance as per ASME SEC-IX.

Regards
Shadab Alam Ansari
Welding Engineer
Olayan Descon

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...