Dear All,
 
I have two more doubts , wether we are adding Si and Al in its pure form or some other compounds form which contains Si and AL abundantly?Are we performing killing operation after making steel(ie, First steel making ,second killing operation) or during steel making process everything happening(ie, steel making and killing happening at the same time with same process)?
 
 
Thanks and Regards
 
 
On Tue, Jun 15, 2010 at 3:19 PM, Prabhu Kumar L <l.prabhukumar@saipem-india.com> wrote:
Dear Limesh,



Silicon & Aluminum are called as deoxidizing elements, which will be
added during steel making process for deoxiding and grain refining
purpose. Based on the need for end product it can be added together or
individual element.



Killed steel: De-oxidation or killing is a process by which strong
deoxidizing element is added to the steel to react with the remaining
oxygen (oxygen used of melting purpose) in the liquid bath to prevent
any further reaction between carbon and oxygen.  Si & Al are high
affinity for oxygen and hence produce oxides such as Al2O3 & SiO2 which
will be removed from top of the steel ingot. This would eliminate the
carbon boil (CO2, CO) and killing the heat and hence the required % of
Cabon is retained in the steel.



Basically pure Oxygen is used for purpose of steel making process which
is called basic oxygen furnace.



Si Killed steel: This type of steel shall have coarse grain structure
(grain no. 1 to 5) and will not react for grain refinement.



Al Killed steel: This will act as deoxidizing and grain refinement as
well and then the structure will be fine grain ie. grain no. 6 & above.
Al will react with Nitrogen to form aluminum nitride to initiate the new
grains at grain boundaries and hence more grains will be formed ie. fine
grains. For notch toughness requirements, steel shall have fine grain
size and hence it will be treated with Al.



Si & Al killed steels: This type of steel called silicon killed, fine
grain. The later is achieved by addition of Al.



Hope it clarifies.



Regards,



L. Prabhu kumar,

Sr. Principal Engineer,



Equipments & Materials Dept.,

Saipem India Projects Limited,

Nungambakkam High Road, Chennai - 600 034, India.

Tel:+91 44 43906588, Ext.: 588, Fax:+91 44 66840345,

Mobile Ph. No.: +91 9003010978.



-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of limesh M
Sent: Tuesday, June 15, 2010 2:05 PM
To: Materials & Welding
Subject: [MW:5599] Silicon&Aluminium Killing



Dear All,



What is meant by Silicon&Aluminium killing of steel?Is there any

significant difference between both process and resulting quality of

material like grain size and other metallurgical property?



Thanks and Regards



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at
http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.






-------------------------------------------------------------------------------------------------------------------------------------------------------------------
DISCLAIMER: The information contained in this communication is intended solely for the use of the individual or
entity to whom it is addressed and others authorized to receive it. It may contain confidential or legally privileged
information. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution
or taking any action in reliance on the contents of this information is strictly prohibited and may be unlawful. If
you have received this communication in error, please notify us immediately by responding to this email and then
delete it from your system. Saipem India Projects Limited (SIPL) is neither liable for the proper and complete
transmission of the information contained in this communication nor for any delay in its receipt.
-------------------------------------------------------------------------------------------------------------------------------------------------------------------

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...