Monday, June 14, 2010

RE: [MW:5581] NONESSENTIAL OR SUPPLEMETARY

Supplementary essential variables shall become mandatory when impact testing is required by design. and when there is a change requalification is required.

Non Essential variables may be revised on WPS, but requalification is not necessary.


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ali Asghari
Sent: Sunday, June 13, 2010 10:46 PM
To: materials-welding@googlegroups.com
Subject: [MW:5580] NONESSENTIAL OR SUPPLEMETARY

Dear All
in QW 250-QW280  in ASME sec IX,SOME VARIABLES ARE NON ESSENTIAL & SUPPLEMENTARY IN SAME TIME.e.g in current
WHICH ONE SHALL BE CONSIDERED?HOW INTERPRETED?
REGARD ADVANCES


No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...