Sunday, June 13, 2010

Re: [MW:5579] swsi IQI wire

Dear kk,

you have achieved higher sensitivity which was very good,

so no need to wory at all.

Regards
kalyan

On Sun, Jun 13, 2010 at 1:29 PM, krishna <wiqw@rediffmail.com> wrote:
HI frnds,
Here we have a job of wall thickness of 11mm (SWSI) we are using IQI 10 ISO 16.
so for 2 % sensitivity 11x2% =0.22
if we see the chart of wire type IQI there is no 0.22 wire dia but
while review of film we see 4th wire i.e 0.20 so is it acceptable or not.
thnx,
kk

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...