Thursday, June 10, 2010

Re: [MW:5503] RE: 5437] Hardness of Untempered Martensite

Hi Prabhu,
 
Thanks for the response.
 
I would like to know that, what will be the hardness value , which is the indication of, presence of the untempered Martensite in Q& T Steel
 
And
 
What will be the morphology of the Microstructure.
 
Is there any specs. or stds ?
 
Regards,
 
K.Babu
Singapore
 
----- Original Message -----
Sent: Wednesday, June 09, 2010 2:05 PM
Subject: [MW:5478] RE: 5437] Hardness of Untempered Martensite

Dear Babu,

 

Untempered Martensite is brittle in nature, which will have high hardness level. Martensite will be formed in carbon and low alloy steel, when the cooling rate is higher than the critical cooling rate. For example, quenching the steel into water/oil from austenitizing temperature range will produce martensite (brittle) structure at room temperature. In order to convert brittle martensite to less brittle and also to retain toughness, tempering process shall follow after quenching

 

During quenching, some % of austenite may retain to room temperature due to some of the alloying elements (austenitic stabilizing elements such as Mn, Ni, C) and cooling rate. This austenite may try to convert as secondary martensite when tempering treatment is carried out. Hence this martensite is called "untempered martensite" which is brittle in nature. This may contribute to the overall brittleness to the material/ structure.

 

Microstrural analysis can reveal the untempered martensite in the steel micro-structure.

 

Regards,

 

L. Prabhu kumar,

Sr. Principal Engineer,

 

Equipments & Materials Dept.,

Saipem India Projects Limited,

Nungambakkam High Road, Chennai - 600 034, India.

Tel:+91 44 43906588, Ext.: 588, Fax:+91 44 66840345,

Mobile Ph. No.: +91 9003010978.


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kathalingam Babu
Sent: Tuesday, June 08, 2010 6:21 AM
To: materials-welding@googlegroups.com
Subject: [MW:5437] Hardness of Untempered Martensite

 

Hi

 

Any body have the idea on hardness for the untempered Martensite ?

 

What will be the morphology of micro?

 

Thanks & Regards,

 

K.Babu
Singapore

 

 

 

 




-------------------------------------------------------------------------------------------------------------------------------------------------------------------
DISCLAIMER: The information contained in this communication is intended solely for the use of the individual or 
entity to whom it is addressed and others authorized to receive it. It may contain confidential or legally privileged 
information. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution 
or taking any action in reliance on the contents of this information is strictly prohibited and may be unlawful. If 
you have received this communication in error, please notify us immediately by responding to this email and then 
delete it from your system. Saipem India Projects Limited (SIPL) is neither liable for the proper and complete 
transmission of the information contained in this communication nor for any delay in its receipt. 
-------------------------------------------------------------------------------------------------------------------------------------------------------------------

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...