HI
IT IS NOT ALLOWED BECAUSE IN WPS 2G NOT COVER 3G SO YOU HAVE NOT QUALIFIED WPS IN 3G POSITION
H.KASHKOUSHA
From: Kaushik Patel <checkspatel@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tue, June 8, 2010 7:48:44 AM
Subject: [MW:5437] Welder Qualification in 2G - 3G
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
IT IS NOT ALLOWED BECAUSE IN WPS 2G NOT COVER 3G SO YOU HAVE NOT QUALIFIED WPS IN 3G POSITION
From: Kaushik Patel <checkspatel@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tue, June 8, 2010 7:48:44 AM
Subject: [MW:5437] Welder Qualification in 2G - 3G
Dear friend,
I have a query as below.
Our customer had establised a WPS/PQR in 2G position - 16 mm thk plate.
They want qualification test for welders in 3G position (6mm Thk Plate), Can we allow the same?
Electrode: E7018
Coupen : IS 2062 Gr. B plate
Ref. Code : AWS D1.1
Regards,
Checks
-- To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment