Sunday, June 6, 2010

Re: [MW:5413] ASME IX

Mr. Ali,
Good morning,
Please note that thermal cutting is not required for multiple specimens prepared from test coupons with thickness more than 25 mm.

As per QW-462.1 a, note that parallel weld lenght of redcuced section is prepared by machining even though edges are thermally cut.

Machining does not affect the machanical properties of metals compared to termal cutting.

Hope this will clarify.

Kind regards.

John Rodrigues


On Sat, 05 Jun 2010 22:44:46 +0530 wrote
>Dear All
I have some inquiries about ASME IX:
1-for prepration of tensile test , thermal cuttuing according to QW-151.1(D)is not permitted, but in QW-462.1
is permitted.please clarify it.
2-if we have a test coupon3/4" thick with GTAWat the root (1/16") and the rest of the test SMAW E7018(11/16").now for preparing turned speciemen maybe part of GTAW is removed, is it permitted?
regards






--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>



John Rodrigues

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...