Ali,
If you are planning to do tensile test, both GTAW and SMAW processes shall be covered.
Regards.
John
On Sat, 05 Jun 2010 22:44:46 +0530 wrote
>Dear All
I have some inquiries about ASME IX:
1-for prepration of tensile test , thermal cuttuing according to QW-151.1(D)is not permitted, but in QW-462.1
is permitted.please clarify it.
2-if we have a test coupon3/4" thick with GTAWat the root (1/16") and the rest of the test SMAW E7018(11/16").now for preparing turned speciemen maybe part of GTAW is removed, is it permitted?
regards






--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>



John Rodrigues

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...