Re: [MW:5400] spec DEP 31.38.01.31

Hi,
           This requirement is not mandatory and applicable for the below cases
1. For Carbon steel Dia 2" (DN-50) and less the welding(all passess) shall be TIG welding
2. For stainless steel piping without back welding of the internal side, the root pass
shall be carried out by the GTAW process with an inert gas purge which shall be
maintained until completion of the second pass. 





(wherever you can not make sound weld (back chipping/back gouging)on root side it's mandatory to go for GTAW root welding.
For stainless steel piping without back welding of the internal side, the root pass
shall be carried out by the GTAW process with an inert gas purge which shall be
maintained until completion of the second pass.

vaithiyanathan,

On Fri, Jun 4, 2010 at 1:27 PM, nixon joseph <nixonjosephq@rediffmail.com> wrote:
Hi

As per shell spec DEP 31.38.01.31 for shop fabrication TIG for root welding is a compulsary requirement?

Regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Best Regards

B.Vaithiyanathan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...