RE: [MW:5370] Hardness requirement for P1 material

Code of construction is B 31.3 & Sec VIII Div.1. There is no H2 / NACE
service in system.

Thanks & Regards,
DHARMESH MISTRY

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of
raghurambathula@gmail.com
Sent: Wednesday, June 02, 2010 10:43 PM
To: materials-welding@googlegroups.com
Subject: RE: [MW:5354] Hardness requirement for P1 material

What is your code of construction?
For e.g. If it is B31.3, refer PWHT table. Else if NACE is applicable,
refer NACE std also.
Sent from my Nokia phone
-----Original Message-----
From: Dharmesh Mistry
Sent: 02/06/2010 1:56:10 pm
Subject: [MW:5351] Hardness requirement for P1 material

Dear all,

Please let me know where I can find hardness requirement for P1
materials.

Thanks & Regards,

DHARMESH MISTRY

Direct : +91 22 6774 0074

Cell +91 98207 35814

Dharmesh.Mistry@heurtey.in

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...