RE: [MW:5361] ask for chemical composition sa-105

Dear Peyman,

these elements shall ( must) be mentioned in the material test certificate, even if they are of zero% content,
if they are not mentioned in the MTC, SO, This material is rejected.

QA/QC ENG: AMR SOLIMAN
PETROJET-EGYPT


Date: Wed, 2 Jun 2010 12:26:21 +0530
From: ravimenakath@yahoo.co.in
Subject: Re: [MW:5348] ask for chemical composition sa-105
To: materials-welding@googlegroups.com

Dear Peyman,
 
The sum of Ni,Cr,Mo,Cu,and Vanadium should not exceed 1.00% . So to calculate this these details needed.
 
Thanks.
 
V.Ravishanker,
 
Senior QA/QC Engineer,
Bahrain
 
 

 


From: peyman behnood <pkhazraei@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Tue, 1 June, 2010 11:59:21 AM
Subject: [MW:5330] ask for chemical composition sa-105

i would be thankful if answer to my question:
,as ASTM_ A105 are the elements Ni, Cr,Mo, Cu, Nb  essential elements
or not  .
I means in the material certificate ,the chemical composition for
above elements  necessary must  be report or not??

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Hotmail: Free, trusted and rich email service. Get it now.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...