Wednesday, June 2, 2010

Re: [MW:5355] Presure Gauge Limits

Dear All,
Thank you for your inputs. I will get the gauge 0-6000.
 
Regards,
S.Senthilkumar 

--- On Wed, 2/6/10, GOPU NAIR <gopunair5343@yahoo.com> wrote:

From: GOPU NAIR <gopunair5343@yahoo.com>
Subject: Re: [MW:5346] Presure Gauge Limits
To: materials-welding@googlegroups.com
Date: Wednesday, 2 June, 2010, 9:51 AM

Dear Sentil Kumar
 
Please read ASME Sec VIII Div.1 UG-102.
UG-102(b) states
 
" Dial indicating pressure gages used in testing shall be graduated over a range of about double the intended maximum test pressure, but in no case shall the range be less than 1.5 nor more than 4 times that pressure". 
 
This means that the gage used for testing 3000 psig shall have a range of 0 to 4500psi or 0 to 12000psi. Ideally the gage must have a range 0 to 6000psi
 
Gopu

--- On Wed, 2/6/10, AGUSTIN JIMENEZ <agumarca@yahoo.com> wrote:

From: AGUSTIN JIMENEZ <agumarca@yahoo.com>
Subject: Re: [MW:5341] Presure Gauge Limits
To: materials-welding@googlegroups.com
Cc: "INSPECTORES DE EQUIPOS ESATICOS" <inspectores_equipos_estaticos@gruposyahoo.com>
Date: Wednesday, 2 June, 2010, 6:16 AM

Hi.Senthilkumar
Is good 4000 psi, the pressure test is better that is in minimun 30% and maximun 70% gauge range.
 
Agustin Jimenez


De: "raghurambathula@gmail.com" <raghurambathula@gmail.com>
Para: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Enviado: mar, junio 1, 2010 10:13:08 AM
Asunto: RE: [MW:5334] Presure Gauge Limits



Sent from my Nokia phone
-----Original Message-----
From: SENTHILKUMAR SWAMINATHAN
Sent:  01/06/2010 2:52:07 pm
Subject:  [MW:5332] Presure Gauge Limits

Dear All,
 
One of the fire water line to be hydrotest in 3000 ksi, with me available gauge is 4000ksi.
 
Is there any documents says we can use this limit gauge for testing or shall be tested only with min 6000ksi gauge only?
 
Regards,
S.Senthilkumar
Angola

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,   Please see the response below.   Regards.   P. Goswami, P. Eng, IWE.   From: materials-welding@googlegroups.com <materials-weld...