Tuesday, June 1, 2010

Re: [MW:5338] ask for chemical composition sa-105

Dear Peyman,
How are you.
there is no defination like essential elements.Whatever the elements mentioned in table 1 of SA 105, all you need to mention in MTC and you need to take care of footnote also. If mfr. wants to mention less elements than required then mfr. has to take prior approval from enduser.

With Regards,
Rutvik
Sr.Surveyor
TATA Projects Ltd.

--- On Tue, 1/6/10, peyman behnood <pkhazraei@gmail.com> wrote:

> From: peyman behnood <pkhazraei@gmail.com>
> Subject: [MW:5330] ask for chemical composition sa-105
> To: "Materials & Welding" <materials-welding@googlegroups.com>
> Date: Tuesday, 1 June, 2010, 2:29 PM
> i would be thankful if answer to my
> question:
> ,as ASTM_ A105 are the elements Ni, Cr,Mo, Cu, Nb 
> essential elements
> or not  .
> I means in the material certificate ,the chemical
> composition for
> above elements  necessary must  be report or
> not??
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members
> personel views and meant for educational purposes only,
> Users must take their own decisions w.r.t. applicable
> code/standard/contract documents.
>


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...