[MW:5668] FCAW Process for welding of tanks

Dear All,
 
We are planning to introduce Flux cored Arc welding for L seams and C seam welding of Tanks.  The Tank dia is 12m and material is ASTM A 515 Gr. 60.  We are planning to use E 71T1 flux cored wires.  FCAW was never used for welding my cleint jobs.  So he is asking history on usage FCAW wires for Tanks, repair percentage, bead apperance and any other adavantages.  If  you have FCAW wire please send me the above details and also photos of  some weld joints also.
 
Regards
 
N.V. PRASAD

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...