Dear KK,

 

As you have seen the 4th wire of ISO 10 to 16 you have achieved 1.8% sensitivity which is above 2% sensitivity. It is acceptable.

 

 

Thanks & Regards

 

Ajithkumar.K

Head of QA/QC Department ( Fabrication Division)

OGASCO L.L.C

Mobile : 0502239844

Tel        : 025500300 Ext.414

Fax       : 02 5500400

Mail     : qcfab@ogasco.ae

Web     : www.ogasco.ae

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of krishna
Sent: 13 June 2010 11:59
To: materials-welding@googlegroups.com
Subject: [MW:5570] swsi IQI wire

 

HI frnds,
Here we have a job of wall thickness of 11mm (SWSI) we are using IQI 10 ISO 16.
so for 2 % sensitivity 11x2% =0.22
if we see the chart of wire type IQI there is no 0.22 wire dia but
while review of film we see 4th wire i.e 0.20 so is it acceptable or not.
thnx,
kk

Image removed by sender.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...