Wednesday, June 9, 2010

[MW:5501] POAK MRKS ON SAW WELDING

Hi

 

We are continuously facing problem of Poak marks on the SAW Welding surface. Welding Consumable L-61 (wire) with 865 (flux) combinations. Any body has idea to prevent this. Please share.

 

Best Regards

 

M.Masthan

K.S.A

 

 

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...