Monday, May 10, 2010

RE: [MW:5124] INFORMATION

Good Morning,

 

Thanks for your reply. I am confused guys. Kindly note the following;

 

·         Below mail from Mr. Rutvik states that St 52.3 according to edition EN10025-2 converted to S355J0.

·         While a mail from Mr. Hermen Pieper states two specs. EN 10210 & EN 10219 in which St 52.3 is called S355J0H or S355J2H.

 

Friends I am confused. Please can you clarify the above since I have to float tender for 850MM, 750MM, & 650MM with Dia; 19MM, 25MM, Length 12 Mtrs.  Floating and Shore Line Pipes which is a high value tender.

 

Your swift response will be appreciated.

 

Thanks in advance for your cooperation.

 

 

With best Regards,

 

Shiraz Parvez

Procurement Coordinator

[Supply & Purchaing Department]

 

National Marine Dredging Company

 

NMDC works for development ...

 

P.O. Box 3649 - Abu Dhabi - U.A.E.

Tel;  +971 2 5516000/418 

Fax; +971 2 5510703

Mob; +971-50-864-4188

Web:  www.nmdc.com

 

P Please consider the environment before printing this email

 

This message (including any attachments) contains confidential information intended for a specific individual and purpose, and is protected by law. If you are not the intended recipient, you should delete this message and are hereby notified that any disclosure, copying, or distribution of this message, or the taking of any action based on it, is strictly prohibited.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of rutvik dixit
Sent: Sunday, May 09, 2010 9:39 PM
To: materials-welding@googlegroups.com
Cc: Khalid Al Amri; TAG Saleh; Ahmed Al Jabir; Hassan
Subject: Re: [MW:5120] INFORMATION

 

Hi Shiraz,
You are talking about Non alloy structural steel st 52.3 German grade. This grade was under EN 10025 -93 edition. As per my knowledge 2004 edition is current edition for EN 10025-2 and  in which for st 52.3U( old grade) converted to S355J0 ( Impact at 0 deg.C) and for st 52.3N     ( old grade) converted to S355J2(Impact at -20 deg.C)

Here S denotes structural steel and 355 denotes its yield strength.

I have inspected this material in plate form at various steel plants.

With Regards,
Rutvik
Sr.Surveyor
TATA Projects Ltd.



--- On Sun, 9/5/10, Shiraz Parvez <spk@nmdc.ae> wrote:


From: Shiraz Parvez <spk@nmdc.ae>
Subject: [MW:5112] INFORMATION
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Cc: "Khalid Al Amri" <kaa@nmdc.ae>, "TAG Saleh" <tsa@nmdc.ae>, "Ahmed Al Jabir" <aaj@nmdc.ae>, "Hassan" <hab@nmdc.ae>
Date: Sunday, 9 May, 2010, 11:44 AM

Good Morning,

 

I have been informed by one of my suppliers dealing in Floating & Shore line pipes that Grade St 52.3 is discontinued and replaced. Can I have more details on this issue? It is very important. And can you provide detaisl on the substitute.

 

 

With best Regards,

 

Shiraz Parvez

Procurement Coordinator

[Supply & Purchaing Department]

 

National Marine Dredging Company

 

NMDC works for development ...

 

P.O. Box 3649 - Abu Dhabi - U.A.E.

Tel;  +971 2 5516000/418 

Fax; +971 2 5510703

Mob; +971-50-864-4188

Web:  www.nmdc.com

 

P Please consider the environment before printing this email

 

This message (including any attachments) contains confidential information intended for a specific individual and purpose, and is protected by law. If you are not the intended recipient, you should delete this message and are hereby notified that any disclosure, copying, or distribution of this message, or the taking of any action based on it, is strictly prohibited.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...