Dear vi jay
Your client is right. You should have ensured client specification before starting the design exercise. There should be a minimum CA considered in the design which will not impart any strength.
Refer cl 5.3.2 of API 650 (guess API is your design code)
Hrishi
Dear All,
Please clarify me the below.
We designed a Tank and send for approval to the client. As per the code there is nothing mentioned about corrosion allowance. As per the tender spec. there is nothing mentioned about corrosion allowance. We got this below reply from engineer.
Kindly help Us.
Regards,
Vijay.
Advanced Oilfield Technology Company LLC,
Muscat.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Your client is right. You should have ensured client specification before starting the design exercise. There should be a minimum CA considered in the design which will not impart any strength.
Refer cl 5.3.2 of API 650 (guess API is your design code)
Hrishi
Sent on my BlackBerry® from Vodafone Essar
From: Vijay <k.vijayaraj@gmail.com>
Date: Thu, 6 May 2010 20:44:24 +0400
To: <materials-welding@googlegroups.com>
Subject: [MW:5095] Corrosion Allowance for Tank Design as per BS14015:2004
Dear All,
Please clarify me the below.
We designed a Tank and send for approval to the client. As per the code there is nothing mentioned about corrosion allowance. As per the tender spec. there is nothing mentioned about corrosion allowance. We got this below reply from engineer.
It is normal practice to provide 3 mm corrosion allowance on shell & base and 1.5 mm for roof material. The requirement is usually from Clients project specifications.
In the present case there is no concern related to Shell as provided thickness is more than actual required thickness plus corrosion allowance. But for the base and roof material no corrosion allowance is available / considered.
As we do not know, if, there are any company project specifications to be followed,
Based on confirmation we will proceed to review and comment the drawing..
Kindly help Us.
Regards,
Vijay.
Advanced Oilfield Technology Company LLC,
Muscat.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments